PRODUCT NAME :
alloy structure steel
STANDARD:
GB/T3077-1999 EN10083-1 EN10083-3 ISO 683-1
GRADE COMPARISION:
GB |
ГОСТ |
ASTM |
BS |
JIS |
NF |
DIN |
40Cr |
40X |
5140 |
520M40 |
SCr440 |
42C4 |
41Cr4 |
ULTRASONIC STANDARD:
GB/T6402-2008 / SEP921-84. ASTM A388
CHEMICAL COMPOSITION;
C |
Si |
Mn |
P≤ |
S≤ |
Cr |
0.37/0.44 |
0.17/0.37 |
0.50/0.80 |
0.035 |
0.035 |
0.80/1.10 |
HEAT TREATMENT SPECIFICATION & MECHANICAL PROPERTIES:
Critical point approximate :Ac3=780℃
Normalizing temperature :850~870℃,hardness 179~229HBS。
Cold pressing workblank softening process :
Temperature 740~760℃,soaking time 4~6h and then by 5~10℃/h cooling , cooling to ≤600℃, out furnace and air cooling .
Quenching temperature 850℃ ±10℃, oil cooling , tempering temperature 520℃±10℃.coolant water / oil
DELIVERY CONDITION :
Forged and slow cooling . If need heat treatment should be indicated in contract .
DIMENSION : mm
ROUND STEEL BAR |
COIL ROD |
WIRE |
SQUARE/ FLAT |
FORGED BAR |
ROLLED BAR |
HOT ROLLED |
COLD DRAW |
FORGED |
ROLLED |
80-650 |
16-250 |
∮5.5-20 |
∮0.2-13 |
120-800×120-800 |
5-38×44-150 10-90×60-305 |
APPLIED RANGE:
The steel after quenched & termpered used in make bearing moderate duty and moderate speed machine parts. Such as knuckle
of automobile, back axle shaft ,and gear , shaft ,worm spline shaft , center sleeve of machine tool .
REMARK:
Above listed parameters and sepcification only for reference . Specific parameters according to standard. Requirments beyond standard
will be negotiated by both sides
.
Delivery state:annealed, spheroidal annealed, quenched & tempered ,bright bar, cold-drawn, etc.
Listed specifications are only typical grades; products of required specifications can be developed/produced as per international, Chinese
or industry standards, or
based on agreements with customers.